Why Do Internal and External Folding Defects Form During Piercing and Rolling?

Internal and external folding defects are the most common and destructive structural flaws in hot-rolled seamless steel pipe production, primarily generated during rotary piercing and continuous rolling stages. Unlike superficial surface scratches that can be repaired by polishing, folding defects are layered metal separation structures that permanently damage the integral continuity of the pipe wall. These defects are invisible in the early production stage and will gradually expand into macroscopic cracks, leakage points and structural failure under long-term high pressure, alternating loads and temperature fluctuations. Most pipeline safety accidents and product rejection issues of seamless pipes are closely related to unregulated folding defects. Based on hot rolling metallurgical principles and industrial production experience, this article analyzes the formation mechanisms, key inducing factors and engineering hazards of internal and external folding defects through question-based subheadings, providing technical guidance for production optimization and quality control.
What Are the Morphological Characteristics of Internal and External Folding Defects?
Internal and external folding defects have distinct morphological features that help distinguish their formation stages and root causes. External folding defects mainly appear as continuous or intermittent spiral creases, linear folds and local metal lamination on the outer surface of seamless pipes. Most external folds are distributed along the rolling direction with uneven depths and irregular edges, which can be partially identified by professional surface inspection and manual screening. In severe cases, external folds run through the entire pipe length, forming obvious layered depressions that damage surface flatness and structural integrity.
Internal folding defects are concealed inside the pipe wall and inner surface, mostly presenting fish-scale or serrated spiral textures. Completely invisible to naked-eye observation, internal folds form tiny layered gaps between inner metal tissues. These hidden defects do not affect the pipe's appearance but severely weaken the wall thickness uniformity and integral mechanical strength. Both internal and external folds belong to irreversible metal tissue damage; once formed, they cannot be eliminated by subsequent heat treatment, straightening or finishing processes, resulting in direct product scrapping in high-standard engineering applications.
How Do Piercing Process Parameters Trigger Internal Folding Defects?
The rotary piercing stage is the core link for internal fold generation, and unreasonable process parameter matching is the leading cause of hidden internal folding defects. Piercing temperature deviation is the primary inducing factor. Excessively high billet heating temperature or prolonged high-temperature holding time leads to excessive metal plasticity and disordered internal metal flow during piercing. The central metal of the billet is repeatedly stretched and squeezed by the piercing mandrel and rolls, forming staggered laminated structures and fish-scale internal folds. In contrast, insufficient piercing temperature reduces metal ductility, causing uneven deformation and local metal accumulation that further aggravate inner wall folding.
Unreasonable equipment adjustment parameters also accelerate internal fold formation. Improper roll inclination angle, mismatched roll gap and worn piercing mandrel will cause unbalanced axial and radial force on the pipe blank during piercing. The mandrel eccentricity and surface abrasion lead to irregular friction and extrusion on the inner metal, breaking uniform deformation rhythm. In addition, excessive single-pass reduction before piercing disrupts the stable metal flow field, making the central tissue prone to separation and folding. These parameter deviations amplify tiny metallurgical flaws in raw billets into complete internal folding defects.
What Raw Material and Pre-Process Flaws Induce External Folding?
Most external folding defects originate from raw material defects and unstandardized pre-treatment processes before rolling. Unprocessed steel billets with residual oxide scales, surface burrs, sharp edges and subcutaneous inclusions are the main inducements of external folds. During high-temperature rolling, hard oxide scales and protruding burrs hinder smooth metal flow, causing local metal accumulation and tensile wrinkling on the pipe surface. Heterogeneous non-metallic inclusions in the billet create local stress concentration points, disrupting continuous metal deformation and forming layered external folds along the rolling direction.
Defective billet surface finishing further exacerbates external folding risks. Billet surface cracks, pits and uneven grinding marks will be stretched and expanded during hot rolling, evolving into continuous spiral external folds. Many manufacturers save costs by omitting high-pressure descaling and billet polishing procedures, leaving residual surface defects. These minor pre-process flaws are continuously amplified in the rolling deformation process, eventually forming large-area external folding defects that fail product quality inspection and engineering acceptance standards.
How Do Rolling Equipment and Operational Errors Aggravate Folding Defects?
Equipment precision attenuation and irregular rolling operation are critical intermediate factors that worsen internal and external folding defects. Long-term operation leads to roll wear, guide plate abrasion and center line misalignment of rolling mills, resulting in unstable rolling gaps and asymmetric extrusion force. During continuous rolling, unbalanced circumferential force causes partial metal overflow and stacking on the pipe surface, forming irregular external folds. Worn guide equipment produces friction scratches and local metal extrusion, which gradually deform into folded structures under repeated rolling pressure.
Unstable rolling rhythm and unreasonable speed matching also induce folding defects. Mismatched rotating speed between piercing rolls and finishing rolls causes asynchronous metal stretching and compression, leading to internal tissue delamination and hidden internal folds. In addition, poor equipment lubrication increases surface friction resistance, hinders uniform metal flow, and intensifies local metal accumulation and wrinkling. These equipment and operational problems turn controllable minor flaws into serious structural folding defects, greatly reducing the finished product qualification rate.
What Engineering Hazards Do Uncontrolled Folding Defects Bring?
Internal and external folding defects bring multi-dimensional irreversible hazards to pipeline engineering operation. Structurally, layered folding defects destroy the integral uniformity of the pipe wall, forming permanent weak links with reduced pressure-bearing capacity and fatigue resistance. Under high internal pressure and alternating fluid scouring, fold tips generate severe stress concentration, easily inducing crack initiation and rapid propagation, which further leads to pipeline wall rupture and medium leakage.
In corrosive service environments, fold gaps become enclosed spaces for moisture and corrosive media accumulation, accelerating stress corrosion and hydrogen-induced cracking. For high-standard projects such as boiler pipelines, petrochemical process pipelines and deep-well oil and gas transmission pipelines, folding defects directly cause product rejection and project unqualified acceptance. In long-term service, unremoved folding defects will shorten pipeline service life by more than 30%, triggering frequent maintenance and even safety accidents, bringing huge economic losses and operational risks to engineering projects.
How Does Hebei Huayang Eliminate Piercing and Rolling Folding Defects?
Hebei Huayang Steel Pipe Co., Ltd. has established a full-process prevention and control system targeting internal and external folding defects caused by piercing and rolling process errors, effectively solving the quality pain points of traditional hot-rolled seamless pipe production. In raw material control, the company implements strict billet pre-inspection and full-scale finishing, thoroughly removing surface oxide scales, burrs and defective billets with internal inclusions to eliminate folding inducements from the source.
In core piercing and rolling processes, Hebei Huayang adopts intelligent parameter calibration systems to precisely control piercing temperature, roll inclination angle and rolling reduction ratio, maintaining stable and uniform metal flow during deformation. Regular equipment maintenance and mandrel polishing eliminate roll wear and center line deviation, avoiding asymmetric extrusion and local metal accumulation. Equipped with full-coverage ultrasonic and radiographic nondestructive testing equipment, the company screens hidden internal folds and superficial external folds one by one, ensuring all delivered products are free of layered structural defects. Through refined process management and strict quality inspection, Hebei Huayang provides high-integrity, defect-free hot-rolled seamless pipes for global high-pressure and high-standard industrial projects.